CT15C
ACI/CAST GRADE | CAST ASTM | CAST EN/DIN | CAST UNS | WROUGHT UNS | WROUGHT GRADE |
|---|
| CT15C | A351 | 1.4859 GX10NiCrNb32-20 | N08151 | – | INCOLOY 800H |
| CHEMICAL COMPOSITION (wt%, TYPICAL VALUES) |
|---|
| C | Cr | Ni | Si | Other |
|---|
| 0.1 | 20.0 | 32.0 | 1.0 | 1.0Nb |
| CASTINGS MINIMUM MECHANICAL PROPERTIES (AT 20°C, UNLESS OTHERWISE SPECIFIED) |
|---|
| Rp0.2[MPa] | Rm [MPa] | A % | Hardness [HB] | Impact [J] |
|---|
| 170 | 435 | 20 | – | – |
| CREEP LIMIT |
|---|
| Creep limit 1% 10.000 hours MPa at °C | Creep strength for 100.000 hours MPa at °C |
|---|
| 600 | 700 | 800 | 900 | 1000 | 1100 | 600 | 700 | 800 | 900 | 1000 | 1100 |
|---|
| 75 | 68 | 42 | 22 | 8 | – | – | 65 | 40 | 21 | 8.5 | – |
| PHYSICAL PROPERTIES (AT 20°C, UNLESS OTHERWISE SPECIFIED) |
|---|
| Microstructure | ρ [kg/dm3] | α [μm/m∙K] (20 – 100 °C) | K [W/m∙K] | Cp [J/kg∙K] | Melting ΔT [°C] |
|---|
| Austenitic, (Carbides) | 8.0 | 14.5 | 11.5 | 460 | 1357-1385 |
| WORKING CONDITIONS / FABRICATION |
|---|
| Heat Treatment | Max working T in air [°C] | Machinability [100 = CF8M] | Patternmaker’s Shrinkage [%] |
|---|
| As Cast | 1050 | – | 2.3 |